Partial thick silver plating repair of crystal holder.
Partial thick silver plating repair
Introduction
Introduction
Polycrystalline silicon experimental furnace
corrosion testing on the surface coating
High temperature test of coating on SUS316L base material
Corrosion test results of SUS316L surface coating against hydrogen chloride gas
The inner wall of the polycrystalline silicon experimental furnace is thickly plated with silver
Polycrystalline silicon crystal growth furnace production line
The inner wall of the polycrystalline silicon crystal growth furnace is thick-silver plated.
The thick silver-plated inner wall enhance the thermal energy effect, resist corrosion and protect the SUS316L furnace body from being corroded by hydrogen chloride gas during the crystal growth process.